The growing demand for sustainable construction materials created a need to investi
gate and identify alternative Supplementary Cementitious Materials (SCMs) that not
only can reduce cement consumption but also promote the utilization of industrial by
products. Among them, steel slag is a calcium and silicate-rich by-product from the
steel industry that was considered as potential to be used as SCM; however, due to its
low reactivity and presence of unstable mineral phase prohibits it from direct applica
tion. So, this study investigates the optimization of the steel slag with mechanical and
chemical treatment methods followed by pH adjustment and carbonation particularly
empahsis on Electric Arc Furnace Slag and Basic Oxygen Furnace Slag. The main
objective was to analyse how different treatment conditions affect mineral dissolution,
carbonate formation, and the potential performance of the treated slag as a partial ce
ment replacement.
Both of the slags were mechanically treated by drying, grinding, and sieving them
through 63 µm before the chemical treatment with 2.5%, 5%, and 10% acetic acid
concentration. The influence was then evaluated through pH monitoring and charac
terization techniques, including ICP-MS, XRD, TGA, SEM, and compressive strength
testing. Subsequent carbonation studies focused mainly on EAF slag under different
carbonation conditions such as 80◦C for 4 hours, 105◦C for 4 hours and 2 hours.
The results demonstrated that increasing the concentration of acid enhances the dis
solution of mineral phases, but XRD analysis indicates the stronger acid treatment also
caused a greater reduction in calcium silicate phases, demonstrating a trade-off between
calcium extraction and preservation of potentially cementitious minerals. Carbonation
results in the formation of crystalline carbonated phases, primarily calcite and arago
nite, which is confirmed by XRD and SEM. TGA showed that the sample carbonated at
80 ◦C for 4 hours showed a greater carbonation-related mass loss among the different
investigated conditions.
Compressive Strength testing with 20% cement replacement further showed that the
sample carbonated at 80 ◦C for 4 hours gained the best 28-day performance among
others, reaching approximately 47 MPa, equivalent to 90% of the reference cement
strength. Overall, the study demonstrates that controlled pre-treatment and mineral
carbonation can improve the potential of EAF slag as SCM. The results also emphasize
that optimum treatment conditions depend on achieving an appropriate balance between
calcium extraction, carbonate formation, preservation of reactive phase, and mechanical
performance.